Percentage remained of PCBs after 2 hours photodegradation under UV light with TiO<sub>2</sub>, graphene-TiO<sub>2</sub> and without catalyst: (a) congener 8; (b) congener 28; (c) congener 30; (d) congener 31; (e) congener 33; (f) congener 74.
- Publication date
- Publisher
Abstract
<p>Percentage remained of PCBs after 2 hours photodegradation under UV light with TiO<sub>2</sub>, graphene-TiO<sub>2</sub> and without catalyst: (a) congener 8; (b) congener 28; (c) congener 30; (d) congener 31; (e) congener 33; (f) congener 74.</p