    Grain boundary electric characterization of Zn7Sb2O12 semiconducting ceramic: A negative temperature coefficient thermistor

    No full text
    The electrical properties of the grain boundary region of electroceramic sensor temperature based on inverse spinel Zn7Sb2O12 were investigated at high temperature. The zinc antimoniate was synthesized by a chemical route based on the modified Pechini method. The electric properties of Zn7Sb2O12 were investigated by impedance spectroscopy in the frequency range from 5 Hz to 13 MHz and from 250 up to 600 degreesC. The grain boundary conductivity follows the Arrhenius law, with two linear branches of different slopes. These branches exhibit activation energies with very similar values; the low-temperature (less than or equal to350 degreesC) and high-temperature (greater than or equal to400 degreesC) regions are equal to 1.15 and 1.16 eV, respectively. Dissimilar behavior is observed on the relaxation time (tau) curve as a function of temperature, where a single slope is identified. The negative temperature coefficient parameters and nature of the polarization phenomenon of the grain boundary are discussed. (C) 2003 American Institute of Physics

    Negative temperature coefficient thermistor based on Bi3Zn2Sb3O14 ceramic: An oxide semiconductor at high temperature

    No full text
    Bi1.5ZnSb1.5O7 dielectric ceramic with pyrochlore structure was investigated by impedance spectroscopy from 400 to 750 degreesC. Pyrochlore was synthesized by the polymeric precursor method, a chemical synthesis route derived from Pechini's method. The grain or bulk resistance exhibits a sensor temperature characteristic, being a thermistor with a negative temperature coefficient (NTC). Only a single region was identified on the resistance curve investigated. The NTC thermistor characteristic parameter (beta) is equal to 7140 degreesC, in the temperature range investigated. The temperature coefficient of the resistance (alpha) was derived, being equal to -4.46x10(-2) degreesC(-1) at 400 degreesC. The conduction mechanism and relaxation are discussed. (C) 2003 American Institute of Physics

    Conductivity mechanism analysis at high temperature in bismuth titanate: A single crystal with sillenite-type structure

    No full text
    Conductivity behavior of the Bi12TiO20 single crystal was investigated by the electric modulus spectroscopy, which was carried out in the frequency range from 5 Hz to 13 MHz and at temperatures higher than 400 degrees C. The resistance curve exhibits a set of properties correlated to a negative temperature coefficient thermistor. In the temperature range investigated, the characteristic parameter (,8) of the thermistor is equal to 4834 degrees C. Temperature coefficients of the resistance (a) were derived being equal to -3.02 x 10(-2) degrees C-1 at 400 degrees C and equal to -9.86 x 10(-3) degrees C-1 at 700 degrees C. The nature of the electric relaxation phenomenon and magnitude dc conductivity are approached. (c) 2005 American Institute of Physics

    Dielectric spectroscopy on Bi3Zn2Sb3O14 ceramic: an approach based on the complex impedance

    No full text
    The dielectric properties and loss of Bi1.5ZnSb1.5O7 a poor-semiconducting ceramic were investigated by impedance spectroscopy, in the frequency range from 5 Hz to 13 MHz. Electric measurements were performed from 100 to 700 degreesC. Pyrochlore type phase was synthesized by the polymeric precursor method. Dense ceramic with 97% of the theoretical density was prepared by sintering via constant heating rate. The dielectric permittivity dependence as a function of frequency and temperature showed a strong dispersion at frequency lower than 10 kHz. The losses (tan delta) exhibit slight dependence with the frequency at low temperatures presenting a strong increase at temperatures higher than 400 degreesC. A decrease of the loss magnitude occurs with increasing frequency. Relaxation times were extracted using the dielectric functions Z(omega) and M(omega). The plots of the relaxation times tau(Z'), and tau(M) as a function of temperature follow the Arrhenius law, where a single slope is observed with activation energy values equal to 1.38 and 1.37 eV, respectively. (C) 2003 Elsevier Ltd. All rights reserved

    ac conductivity and conduction mechanism of NaNbO3 semiconductor antiferroelectric ceramic: A relaxational approach at high temperature

    No full text
    The electric properties of the sodium niobate perovskite ceramic were investigated by impedance spectroscopy in the frequency range from 5 Hz to 13 MHz and from room temperature up to 1073 K, in a thermal cycle. Both capacitance and conductivity exhibit an anomaly at around 600 K as a function of the temperature and frequency. The electric conductivity as a function of angular frequency sigma(omega) follows the relation sigma(omega)=Aomega(s). The values of the exponent s lie in the range 0.15less than or equal tosless than or equal to0.44. These results were discussed considering the conduction mechanism as being a type of polaron hopping. (C) 2003 American Institute of Physics

    Crystallographic properties of KSr2Nb5O15

    No full text
    Nanostructured KSr2Nb5O15 oxide was synthesized by the polymeric precursor method, a chemical synthesis route based on the Pechini's method. The X-ray diffraction (XRD) pattern of the calcined powder at 1150 degreesC were performed in the angular range 5 less than or equal to 20 less than or equal to 120degrees with a 0.02degrees step and a fixed counting time of 30 s. The XRD data were analyzed by the Rietveld refinements using the FullProf software. The results C showed a tetragonal system with the tetragonal tungsten bronze structure (TTB) type (a = 12.4585 (2) Angstrom and c = 3.9423 (6) Angstrom, V = 611,90 (2) Angstrom). In this work, the sites occupancy by the K+ and Sr2+ cations on the TTB type structure were determined. The thermal parameters (B) were analyzed. (C) 2004 Elsevier B.V. All rights reserved

    The effect of heating rate on the sintering of agglomerated NaNbO3 powders

    No full text
    The effect of heating rate on the sintering of agglomerated NaNbO3 powders, processed by the polymeric precursors method, was studied. The results showed that the presence of agglomerated powder leads to a heterogeneous microstructure, with bimodal grain size distribution, after sintering. Using a high heating rate, the sintering of agglomerated particles was inhibits, leading to a homogeneous microstructure, with single grain size distribution. (C) 1998 Kluwer Academic Publishers

    Dielectric properties of Na1-xLixNbO3 ceramics from powders obtained by chemical synthesis

    No full text
    Ultra-fine powders of Na1-xLixNbO3 (x=0; 0.06; 0.09; 0.12) were synthesized by the Polymeric Precursors Method. Such powders had their orthorhombic structures determined by X-ray diffraction and their surface area determined by BET isotherms (less than 10 m(2) g(-1)). Densification was followed by dilatometric study. The powders, calcined at 700 degrees C for 5 h, were sintered at 1290 degrees C during 2 h under ambient atmosphere with no application of extra pressure. The samples with relative densities higher than 95% were analyzed by impedance spectroscopy at room temperature, under a signal amplitude of 1 V-rms. Dielectric constants of about 180 and dielectric loss factor of about 0.03 were measured showing small dependence with frequency. The electrical properties were similar to those obtained for samples sintered by hot pressing. (C) 1999 Elsevier B.V. Limited and Techna S.r.l. All rights reserved