25 research outputs found

    Draft Genome Sequence of Firmicute Strain S0AB, a Heterotrophic Iron/Sulfur-Oxidizing Extreme Acidophile

    Get PDF
    The draft whole-genome sequence of the extremely acidophilic and novel Firmicutes strain S(0)AB is reported. The genome comprises 3.3 Mbp and has a GC content of 43.72%. In total, 3,240 protein-coding genes, 56 tRNA genes, and 11 rRNA genes were predicted

    Approaches for Eliminating Bacteria Introduced during In Situ Bioleaching of Fractured Sulfidic Ores in Deep Subsurface

    Get PDF
    The major objective of the EU Horizon 2020 project “BioMOre” is the technical realization of indirect in situ leaching of Kupferschiefer sandstone and black shale ore by a ferric iron lixiviant generated by a mixed culture of autotrophic, acidophilic, iron-oxidizing bacteria and archaea in a ferric iron-generating bioreactor (FIGB). These organisms could colonize the deeply buried geological formations even under anaerobic conditions as most are able to grow by coupling the reduction of ferric iron to the oxidation of reduced sulfur compounds in the absence of oxygen. Development of an inhibition protocol to eliminate these allochthonous microbial bioreactor populations subsequent to the completion of in situ bioleaching was therefore investigated. Column bioleaching experiments using a laboratory-scale FIGB confirmed not only that metals were solubilised from both the sandstone and shale ores, but also that significant numbers of bacteria were released from the FIGB. The efficacy of 13 different chemical compounds in inhibiting microbial iron oxidation has been tested at different concentrations in shake flask and FIGB-coupled columns. Iron-oxidation activity, microcalorimetrically-determined activity and ATP measurements, in combination with microscopic cell counts and biomolecular analysis (T-RFLP, qPCR), plate counts and most-probable-number (MPN), were used to monitor the inhibiting effects on the acidophiles. Complete inhibition of metabolic activity of iron-oxidizing acidophiles was achieved in the presence of 0.4 mM formate, 300 mM chloride, 100 mM nitrate, 10 mM of primary C6 to C8 alcohols, 100 mM 1-butanol, 100 mM 1-pentanol, 0.1 mM SDS or 0.35 mM benzoic acid. No inhibition was found for 0.6 mM acetic acid and 200 mM methanol. Based on these results a recipe for the chemical composition of the “decommissioning solution” is proposed.</jats:p

    A novel closed-loop biotechnology for recovery of cobalt from a lithium-ion battery active cathode material

    Get PDF
    In recent years, the demand for lithium-ion batteries (LIBs) has been increasing rapidly. Conventional recycling strategies (based on pyro- and hydrometallurgy) are damaging for the environment and more sustainable methods need to be developed. Bioleaching is a promising environmentally friendly approach that uses microorganisms to solubilize metals. However, a bioleaching-based technology has not yet been applied to recover valuable metals from waste LIBs on an industrial scale. A series of experiments was performed to improve metal recovery rates from an active cathode material (LiCoO ; LCO). (i) Direct bioleaching of ≤0.5 % LCO with two prokaryotic acidophilic consortia achieved &gt;80 % Co and 90 % Li extraction. Significantly lower metal recovery rates were obtained at 30 °C than at 45 °C. (ii) In contrast, during direct bioleaching of 3 % LCO with consortia adapted to elevated LCO levels, the 30 °C consortium performed significantly better than the 45 °C consortium, solubilizing 73 and 93 % of the Co and Li, respectively, during one-step bioleaching, and 83 and 99 % of the Co and Li, respectively, during a two-step process. (iii) The adapted 30°C consortium was used for indirect leaching in a low-waste closed-loop system (with 10 % LCO). The process involved generation of sulfuric acid in an acid-generating bioreactor (AGB), 2-3 week leaching of LCO with the biogenic acid (pH 0.9), selective precipitation of Co as hydroxide, and recirculation of the metal-free liquor back into the AGB. In total, 58.2 % Co and 100 % Li were solubilized in seven phases, and &gt;99.9 % of the dissolved Co was recovered after each phase as a high-purity Co hydroxide. Additionally, Co nanoparticles were generated from the obtained Co-rich leachates, using , and Co electrowinning was optimized as an alternative recovery technique, yielding high recovery rates (91.1 and 73.6% on carbon felt and roughened steel, respectively) from bioleachates that contained significantly lower Co concentrations than industrial hydrometallurgical liquors. The closed-loop system was highly dominated by the mixotrophic archaeon and sulfur-oxidizing bacteria and . The developed system achieved high metal recovery rates and provided high-purity solid products suitable for a battery supply chain, while minimizing waste production and the inhibitory effects of elevated concentrations of dissolved metals on the leaching prokaryotes. The system is suitable for scale-up applications and has the potential to be adapted to different battery chemistries

    Microbial processes with the potential to mobilize As from a circumneutral-pH mixture of flotation and roaster tailings

    Get PDF
    The Northwest Tailings Containment Area at the inactive Giant Mine (Canada) contains a complex mixture of arsenic-containing substances, including flotation tailings (84.8 wt%; with 0.4 wt% residual S), roaster calcine wastes (14.4 wt% Fe oxides), and arsenic trioxide (0.8 wt%) derived from an electrostatic precipitator as well as As-containing water (21.3 ± 4.1 mg L−1 As) derived from the underground mine workings. In the vadose zone the tailings pore water has a pH of 7.6 and contains elevated metal(loid)s (2.37 ± 5.90 mg L−1 As); mineral oxidizers account for 2.5% of total 16S rRNA reads in solid samples. In the underlying saturated tailings, dissolved Fe and As concentrations increase with depth (up to 72 and 20 mg L−1, respectively), and the mean relative abundance of Fe(III)-reducers is 0.54% of total reads. The potential for As mobilization via both reductive and oxidative (bio)processes should be considered in Giant Mine remediation activities. The current remediation plan includes installation of an engineered cover that incorporates a geosynthetic barrier layer

    Efficient dealkalization of red mud and recovery of valuable metals by a sulfur-oxidizing bacterium

    Get PDF
    Red mud (RM) is a highly alkaline polymetallic waste generated via the Bayer process during alumina production. It contains metals that are critical for a sustainable development of modern society. Due to a shortage of global resources of many metals, efficient large-scale processing of RM has been receiving increasing attention from both researchers and industry. This study investigated the solubilization of metals from RM, together with RM dealkalization, via sulfur (S(0)) oxidation catalyzed by the moderately thermophilic bacterium Sulfobacillus thermosulfidooxidans. Optimization of the bioleaching process was conducted in shake flasks and 5-L bioreactors, with varying S(0):RM mass ratios and aeration rates. The ICP analysis was used to monitor the concentrations of dissolved elements from RM, and solid residues were analyzed for surface morphology, phase composition, and Na distribution using the SEM, XRD, and STXM techniques, respectively. The results show that highest metal recoveries (89% of Al, 84% of Ce, and 91% of Y) were achieved with the S(0):RM mass ratio of 2:1 and aeration rate of 1 L/min. Additionally, effective dealkalization of RM was achieved under the above conditions, based on the high rates (>95%) of Na, K, and Ca dissolution. This study proves the feasibility of using bacterially catalyzed S(0) oxidation to simultaneously dealkalize RM and efficiently extract valuable metals from the amassing industrial waste