Towards fabrication of ordered gallium nanostructures by laser manipulation of neutral atoms: study of self-assembling phenomena
Surface diffusion has an impact on the lateral resolution of nanostructures
in bottom-up atom nanofabrication. In this paper we study the effects of the
gallium atoms self-assembled on silicon surfaces (100) patterned with trenches
at different slopes. These particular substrate morphologies have been made to
enable an effective deposition rate variation along the surface. In this way we
experimentally mimic the effect of the atomic flux modulation created by
standing wave during an atom nanofabrication experiment. Even if we observe
self organization of gallium atoms on the surface, we conclude that the
nano-islands are not affected by surface diffusion processes and the effective
variation of the deposition rate per unit area is the dominant factor affecting
the growth differences along the surface. This result demonstrates that the
gallium atoms self-organization should not prevent the observation of a
periodic nano-patterning created by atom nano-fabrication techniques.Comment: 7 pages, 5 figures, EMRS conference procee
Correlating electron trapping and structural defects in Al2O3 thin films deposited by plasma enhanced atomic layer deposition
In this article, electron trapping in aluminum oxide (Al2O3) thin films grown by plasma enhanced atomic layer deposition on AlGaN/GaN heterostructures has been studied and a correlation with the presence of oxygen defects in the film has been provided. Capacitance–voltage measurements revealed the occurrence of a negative charge trapping effect upon bias stress, able to fill an amount of charge traps in the bulk Al2O3 in the order of 5 × 1012 cm−2. A structural analysis based on electron energy-loss spectroscopy demonstrated the presence of low-coordinated Al cations in the Al2O3 film, which is an indication of oxygen vacancies, and can explain the electrical behavior of the film. These charge trapping effects were used for achieving thermally stable (up to 100 °C) enhancement mode operation in AlGaN/GaN transistors, by controlling the two-dimensional electron gas depletion
Nanoscale structural characterization of epitaxial graphene grown on off-axis 4H-SiC (0001)
In this work, we present a nanometer resolution structural characterization of epitaxial graphene (EG) layers grown on 4H-SiC (0001) 8° off-axis, by annealing in inert gas ambient (Ar) in a wide temperature range (Tgr from 1600 to 2000°C). For all the considered growth temperatures, few layers of graphene (FLG) conformally covering the 100 to 200-nm wide terraces of the SiC surface have been observed by high-resolution cross-sectional transmission electron microscopy (HR-XTEM). Tapping mode atomic force microscopy (t-AFM) showed the formation of wrinkles with approx. 1 to 2 nm height and 10 to 20 nm width in the FLG film, as a result of the release of the compressive strain, which builds up in FLG during the sample cooling due to the thermal expansion coefficients mismatch between graphene and SiC. While for EG grown on on-axis 4H-SiC an isotropic mesh-like network of wrinkles interconnected into nodes is commonly reported, in the present case of a vicinal SiC surface, wrinkles are preferentially oriented in the direction perpendicular to the step edges of the SiC terraces. For each Tgr, the number of graphene layers was determined on very small sample areas by HR-XTEM and, with high statistics and on several sample positions, by measuring the depth of selectively etched trenches in FLG by t-AFM. Both the density of wrinkles and the number of graphene layers are found to increase almost linearly as a function of the growth temperature in the considered temperature range
Toward A Metal-Free Contact Based On Multilayer Epitaxial Graphene On 4H-SiC
We report on a promising approach to realize bifacial silicon carbide (SiC) based ultraviolet (UV) photodetectors with no metallic electrodes. The ohmic contact regions, consisting of a few conductive carbon-rich layers, while maintaining the necessary UV sensitivity for the photodetector’s operation, are directly realized using a nanosecond-pulsed excimer laser. By combining structural, optical, and electrical characterization, we demonstrate how this treatment allows the formation of ohmic contacts, on both front and rear side, using fluence higher than 1.6 J/cm2 and 3.2 J/cm2, respectively
Ultralow loading electroless deposition of IrOx on nickel foam for efficient and stable water oxidation catalysis
Abstract Photocatalysis and electrolysis are crucial processes for the development of a sustainable, clean energy system, since they enable solar fuel production, such as hydrogen by water splitting, as well as CO2 reduction. In these processes efficient and robust catalysts for water oxidation are required and the reduction of employed amount of noble metals is crucial to reduce costs and increase the sustainability of the technology. To obtain extremely low iridium loading on nickel foam electrodes we have employed electroless deposition by spontaneous galvanic displacement as a simple, low cost, highly scalable technique. After deposition the Ir oxidation has been achieved by annealing in air at 250 °C. By varying the deposition parameters, an optimal condition has been achieved, with an overpotential for water oxidation of 360 mV at 10 mA cm−2 in 1.0 M KOH solution. The Ni foam coverage with Ir oxide has also a positive impact on the electrode stability, strongly decreasing the degradation rate, compared to the case of bare Ni foam. The average amount of noble metal in the best performing electrode is only 35 μg cm−2 for a 1.6 mm thick Ni foam electrode. The proposed approach is highly promising for gas diffusion electrodes, and can be implemented in electrolytic cells, as well as in fuel cells
Nanoporous Ge electrode as a template for nano-sized (<5 nm) Au aggregates
none8In this paper we present the extremely peculiar electrical properties of nanoporous Ge. A full
and accurate electrical characterization showed an unexpected and extremely high
concentration of positive carriers. Electrochemical analyses showed that nanoporous Ge has
improved charge transfer properties with respect to bulk Ge. The electrode behavior, together
with the large surface-to-volume ratio, make nanoporous Ge an efficient nanostructured
template for the realization of other porous materials by electrodeposition. The pores were
efficiently decorated by Au nanoparticles of diameter as low as 1–5 nm, prepared by
electrochemical deposition. These new results demonstrate the potential and efficient use of
nanoporous Ge as a nanostructured template for nano-sized Au aggregates, opening the way
for the realization of innovative sensor devices.openG.Impellizzeri; L.Romano; B.Fraboni; E. Scavetta; F.Ruffino; C.Bongiorno; V. Privitera; M.G.GrimaldiG.Impellizzeri; L.Romano; B.Fraboni; E. Scavetta; F.Ruffino; C.Bongiorno; V. Privitera; M.G.Grimald
Extended defects in 3C-SiC: Stacking faults, threading partial dislocations, and inverted domain boundaries
Abstract The presence of extended bi-dimensional defects is one of the key issues that hinder the use of wide band-gap materials hetero-epitaxially grown on silicon. In this work, we investigate, by STEM measurements and molecular dynamic simulations, the structure of two of the most important extended defect affecting the properties of cubic silicon carbide, 3C-SiC, hetero-epitaxially grown on (001) silicon substrates: (1) stacking faults (SFs) with their bounding threading dislocation arms, even along with unusual directions, and (2) inverted domain boundaries (IDBs). We found that these two defects are strictly correlated: IDBs lying in {111} planes are intrinsically coupled to one or more SFs. Moreover, we observed that threading partial dislocations (PDs), limiting the SFs, appear to have non-conventional line directions, such as [112], [123], and [134]. Molecular dynamics simulations show that [110] and [112] directions allow for stable dislocation structures, while in the unusual [123] and [134] directions, the PDs are composed of zig-zag dislocation lines in the [112] and [110] directions
- …