Mo(Al,Si)2 has been prepared by hot pressing elemental powders of Mo, Al and Si, at 1200-1700xB0;C and 22 MPa. Mo5Si3 or Mo5Si3C have been observed as minor phases in all the samples with 1300xB0;C being the best processing temperature for synthesizing Mo(AlSi)2: with minimum amount of impurities. As the soaking time increases, the amount of impurity phases also increases. xA9; 2001 Elsevier Science Ltd and Techna S.r.l. All rights reserved